The osb is nailed on correctly but is bowing out from the house between studs a good 4 5 inches.
Osb siding problems.
We frame with 2x6 studs 24 o c.
This is not the case nearly as much with the plywood version of t1 11.
Osb s lower quality means that it becomes very vulnerable to moisture.
The most common failure is the appearance of a warp bow or buckle in the sheathing used for exterior walls.
Over time delamination edge checking and buckling are likely to happen as the glue slowly gives up.
The problem was solved by removing the offending soil heap and replacing the rotten timber and osb.
As with most construction failures there is no single smoking gun problem and no silver bullet solution.
The type that really had issues was the lap type made by louisiana pacific lp.
The 7 16 osb sheathing on the sides of the house is buckling so badly it had caused the vinyl siding to unzip itself.
Wood chip siding has been around for many years but in the late 80 s and early 90 s a certain type of osb oriented strand board siding really became popular around salem oregon and the pacific northwest.
Why osb grade t 1 11 siding fails the problem with t1 11 siding however is not with its cost functionality or even the aesthetics.
And cover them with 7 16 osb and then half inch dow blue foam board.
Wood siding will expand and contract in changing weather conditions and when installed tightly no room is allowed for these patterns causing the buckling.